The goal for this weekend is to finish the fascia on the first two modules, using the steam bending approach to get the curve around the end module. Today I ripped the 2x8 foot half sheet of 1/4” MDF I got into four strips, each a hair over 6” wide. The mathematically inclined may be wondering how you can get 4 6” wide strips plus the 3 almost 1/8” wide kerfs out of a 24” wide piece of MDF. I expected to put the last strip in the miscellaneous pile but measured it just to be sure and I actually had to trim a hair off it. A little googling reveals that nominal 4x8 sheets of MDF are often 49x97 to allow for edge trimming. That worked out nicely!
A nice trick I picked up somewhere for drawing a line parallel to the edge of a sheet if you’ve got a number of them you need the same size is to set the combination square at the distance to the line and slide it along the edge.
Four nice 6” x 8’ strips of fascia, with bits of future modules behind them.
I set up the module upside down on the bench and got everything ready for clamping, then fired up the Steam-O-Matic 5000.
The old shop wash cloth keeps the steam from escaping around the edges, without providing a hard surface for condensation that would result in puddles on the MDF. The steam still escapes along the length - the MDF never actually touches the pot.
About 20 minutes of flipping and steaming later it seemed like it was bendier than my test steamed pieces so I carted it in and bent it around the corner. I was extremely annoyed to get a bit of a crack in the middle of the bend. I clamped it all up anyway and I’ll see if it’s useable once it’s had time to cool and dry. The crack is similar the one I got in the first 409 experiment, kind of a shallow diagonal in the outer third of the thickness under where the black clamp is. There’s a piece of sheet metal around the outside of the bend to give it a little support.
![[259338%2F9680716%2Fmceclip0]](https://d28lcup14p4e72.cloudfront.net/259338%2F9680716%2Fmceclip0.png)
So, what went wrong? The steam bend that went well was in a shorter piece, which I could flex a little, steam more, flex a bit more, etc. and slowly tighten up the bend to the amount I wanted. That’s easy to do with a piece 3 or so feet long, but an 8 foot long piece with the bend near one end that’s basically impossible without some much fancier setup. So I waited until I thought it was flexible enough and then did the whole bend in one go. I think if I need to redo this corner I’ll do it with a piece short enough to bend gradually and splice on a second piece to finish the length of the front of the module. It wouldn’t be hard to do a 45 degree scarf with the tracksaw which would probably work pretty well. Doesn’t have the appeal of a single piece, but maybe more practical.
I’ll give this a few hours to cool and dry and then see what it looks like. If it’s not too bad I may try pressing the crack together with some glue in it. It’s just going to be painted, so as long as I can make it strong enough it doesn’t have to be pretty before paint.